Table 1 Alginate gelling formulations teste d

From: Rheological characterization of an injectable alginate gel system

Figure

Sodium alginate

Ca/Sr alginate

Concentration

F G

M W

Concentration

F G

Bound ion

M W

Figure 2 (lower panel)

1.0%

0.70

219 kDa

1.1%

0.65

Sr

130 kDA

1.0%

0.44

222 kDa

1.1%

0.65

Sr

130 kDA

Figure 2 (upper panel)

1.0%

0.70

220 kDa

1.0%

0.47

Ca

176 kDa

1.0%

0.45

222 kDa

1.0%

0.47

Ca

176 kDa

Figure 3

1.0%

0.69

257 kDa

1.1%

0.65

Sr

130 kDA

1.0%

0.69

70 kDa

1.1%

0.65

Sr

130 kDA

2.0%

0.69

70 kDa

1.1%

0.65

Sr

130 kDA

Figure 4

1.0%

0.69

219 kDa

1.1%

0.65

Sr

130 kDA

Figure 5

0.4-1.6%

0.69

219 kDa

0.4-1.6%

0.65

Sr

130 kDA

0.4-1.6%

0.69

219 kDa

0.4-1.6%

0.47

Ca

176 kDa

Figure 6

1.0%

0.69

219 kDa

1.1%

0.65

Sr

130 kDA

Table 2

1.0%

0.45

220 kDa

1.0%

0.47

Ca

176 kDa

1.0%

0.70

222 kDa

1.0%

0.47

Ca

176 kDa